18YF3

18YF3

LLDPE made via Hostalen Process

Film properties are obtained on 25 μ film made on 25 mm blown exturder according to method MA 17313, unless specified. The density corresponds to the basic grade product , after additivation the density is increased depending on the type of additivation. On High Performance (HP) types, density can not be corolated to stiffness in the same way of conventional LLDPE, due to the diffeernt polymer structure.

HDPE: 18YF3
Features
  • Terpolymer HP-LLDPE
Density: 0.918-0.921
Applications
  • Shrink Film
  • High Performance
MFI: 0.35
Additives
  • THERMAL ANOTIOXIDANT

Material properties (This data are typical values and are not to be construed as product specifications)

Test/Composition Unit Typical Value Method
Dart s 220 D1709/A
Density g/ml 918 D 1505
Elmendorf tear, MD g 250 D 1922
Elmendorf tear, TD g 550 D 1922
Elongation at break , MD % - D 882
Elongation at break, TD % - D 882
MFR "E" g/10 min 0.35 D 1238
Haze % 18 D 1003
Gloss 45° 0% 45 D1709/A
Tensile Strenght, MD Mpa - D 882
Tensile Strenght, TD Mpa - D 882
Yield Strength , MD Mpa - D 882
Yield Strength , TD Mpa - D 882
F/E ratio - 32 D 1238
Fish eyes (Gels) No./m2 100 -
Density final g/l 918-921 D 1505
Ti content ppm 2.5 D1925
Y.l - 0 -