LLDPE made via Spherilene Process
HP-LL18XF5 N is a termopolymer of ethylene, propylene & butene-1 for high
strength application especially heavy duty shipping sacks, ice bag, frozen food
bags, potato bags and agriculture films which have good sealability and excellent
puncture resistance. Goods produced from this grade have outstanding toughness,
excellent puncture resistance, good heat sealing behavior and excellent machinability
on conversion lines. HP-LLDPE's process is easier than conventional LLDPEs
and have low gel. HP-LL18XF5 N is a grade without slip additives.
HDPE: HP-LL18XF5/N |
Features |
- Exellent punctuer resistance.
- Exellent machinability on conversion lines.
|
Density: 0.918-0922 |
Applications |
- T-bags & other bags, Food Packaging for frozen products, Agricultural film,
Heat seal film, Food Packaging
|
MFI: 0.5 |
Additives |
- HP-LL18XF5:Thermal Antioxidant/ Anti-blocking/ Slip Agent
- HP-LL18XF5N:Thermal Antioxidant/ Antiblocking Agent
|
Material properties
(This data are typical values and are not to be construed as product specifications)
Resin Properties |
Unit |
Typical Value |
Test Method |
Melt Index |
g/10 min |
0.5 |
D1238 |
Density |
g/cm³ |
0.918 |
D1505 |
Film Properties |
Unit |
Typical Value |
Test Method |
Dart Impact |
g |
125 |
D1709 |
Vicat Softening Point |
°C |
127 |
D1525 |
Tensile Strenght at Yield |
Mpa |
11/10 |
D638 |
Tensile Strenght at Break |
Mpa |
40/35 |
D638 |
Ultimate Elongation |
% |
600/750 |
D638 |
Elmendorf Tear |
g |
240/400 |
D1922 |
Haze |
% |
30 |
D1003 |
Gloss 45° |
|
25 |
D2457 |
Handellling and Health Safety
sMolten polymers could be injured skin
or eye so safety glasses and appropriate gloves are suggested to prevent possible
thermal injuries. Also appropriate ventilation is suggested in working by melt polymer.
Accumulation of fines or dust particles that are in this grade is not suitable because
of explosion hazard probability. So adequated filters and grounding exists at all
time are recommended.
Storage
Polyethylene products (in pelletised or
powder form) should not be stored in direct sunshine and/or heat radiation. Ultraviolet
cause a change in the material properties.The Storage area should be dry and preferably
don't exceed 50 °C. It is
advisable to process PE resin within 6 months after delivery. JPC would not ressponsible about quality diminishing such as color
change, bad smell or ets which caused by bad storage conditions. It is better to
process PE resin within 6 months after delivery
packaging
Jam Polymers Polyolefin resins are supplied
in pllet form packed in 25kg bags. Alternative packaging modes are avalable for
selected grades.